Extrusion Blow Molding Defects and Troubleshooting: Causes, Checks and Corrective Actions

2026-08-28 0 Ka bar min sako
Extrusion Blow Molding Defects & Troubleshooting | Kinggle

Irin wannan lahani na iya fitowa daga guduro, samuwar parison, kayan aiki, iska, sanyaya, yanayin injin ko canjin girke-girke mara izini. Wannan jagorar yana taimaka wa ƙungiyar samarwa ta sami shaida mai amfani ta farko kafin canza saituna.

ByNingbo Kinggle Machinery Co., Ltd. · An buga Agusta 27, 2026

Extrusion blow molding machines assembled inside the Kinggle factory
Amsa da sauri:Kada a gyara lahanin gyare-gyare daga bayyanar shi kaɗai. Ya ƙunshi sassan da ake zargi, yin rikodin sake zagayowar gazawar farko kuma kwatanta tsari tare da ingantaccen tushe. Yanke shawarar ko laifin ya biyo baya gefe ɗaya, rami ɗaya, gyaggyarawa ɗaya, ƙurar guduro ɗaya ko gabaɗayan injin. Bincika kayan aiki, ainihin yanayin zafi, halayen parison, rufewar mold, busa iska da sanyaya kafin canza girke-girke. Canja sauyi ɗaya a lokaci guda, ƙirƙira isassun kewayon don isa ga ingantaccen yanayi, kuma tabbatar da sakamakon tare da nauyin sashi, ma'aunin bango da gwajin aikin da ake buƙata.

Bayanan kalmomi:Ƙungiyoyin samarwa na duniya na iya kiran batu iri ɗayabusa lahani, busa gyare-gyaren matsalolin da mafita, Lalacewar kwalban filastikkobusa gyare-gyaren ɓangaren lahani. Canje-canjen sunan harafin da sashin; hanyar bincike ta tushen shaida ba ta.

Fara da aikin bincike mai Layer huɗu

Jerin dalilai masu yiwuwa yana da amfani, amma kuma yana iya ƙarfafa daidaitawa bazuwar. Mafi kyawun jeri yana taƙaita kuskure daga ɓangaren da ya ƙare baya ta hanyar aiwatarwa. Mai ba da guduro yana jagora dagaLyondell Basell, Formosa FilastikkumaTeknor Apexduk suna nuna cewa alama ɗaya na iya samun tsari da yawa, abubuwa da dalilai na kayan aiki.

1. Ya ƙunshiWare sassan da ake zargi, kare mutane da kayan aiki, da adana ƙararrawa ko samfurin farko.
2. Gano wuriNemo matakin farko da ya canza: abu, extrusion, parison, mold kusa, busa, sanyaya ko kulawa.
3. KwatantaKwatanta ainihin dabi'u da yanayin jiki tare da ingantaccen girke-girke, samfuri mai kyau da tushen amfani na yau da kullun.
4. TabbatarwaYi gyare-gyaren sarrafawa guda ɗaya, jira tsayayyen hawan keke kuma maimaita ma'aunin inganci iri ɗaya.

Yi tambayoyi huɗu kafin a taɓa girke-girke

  1. Shin lahani na gida ne ko na duniya?Bangare ɗaya yana ba da shawarar mutuƙar tsakiya, jeri na ƙira, sanyaya rashin daidaituwa ko huɗawar waje. Kowane rami ko kowane bangare yana nuna abin da aka raba, zazzabi, matsa lamba, mai amfani ko batun jeri.
  2. Shin maimaituwa ne ko na ɗan lokaci?Rashin lahani a matsayi ɗaya kowane zagayowar yana nuni zuwa ga lissafi, kayan aiki ko taron aiki tare. Lalacewar motsi tana nunawa sau da yawa zuwa ga rashin kwanciyar hankali extrusion, gurɓatawa, kayan aiki, ra'ayin firikwensin ko bambancin harbi.
  3. Menene ya canza nan da nan kafin ya bayyana?Bincika yawan kayan abu, yawan regrind, launi, bita ga girke-girke, sabis na gyare-gyare, gyaran dumama, da'irar ruwa, buƙatun iska, canjin canji da yanayin farawa.
  4. Shin ma'aunin ya yarda da hukuncin gani?Kwantena na iya kama da karɓuwa yayin da ƙaramin bango, nauyi, girman wuyansa, aikin ɗigogi ko babban kaya ya ƙaura zuwa wajen abin da aka yarda da shi.
Iyakar aminci:tsayawar inji ko saƙon HMI ba hanya ce ta ware kuzari ba. Kar a shiga wurin da aka tsare, bincika mutuwa mai zafi, share matsi, aiki akan tsarin matsa lamba ko ketare wani kullewa daga wannan labarin. Yi amfani da littafin na'ura, tsarin da aka ba da izini na shuka da kuma doka mai dacewa. A {asar Amirka, ana kula da sarrafa-makamashi mai haɗari da na'uraOSHA 1910.147kumaOSHA 1910.212.

Extrusion busa gyare-gyaren matsala matsala matrix

Yi amfani da wannan tebur azaman hanyar zuwa cak na farko, ba azaman takardar saiti na duniya ba. Matsayin guduro, juzu'i na juzu'i, shugaban mutu, mold, nau'in inji da ƙayyadaddun ƙayyadaddun inganci suna ƙayyade ingantacciyar taga mai aiki.

Lalaci ko kalmar nema Dalili mai yiwuwa yadudduka Shaida ta farko don dubawa Hanyar gyarawa
Fish mai yawa Abubuwa da yawa a cikin tsunkule, ƙirar da ba ta cika rufewa ba, batun matsawa, lalacewa ko lalacewa ko tsinkewa, jeri ko lokaci Wurin walƙiya da kauri, wuri-kusa-ƙusa, ra'ayin manne, nauyin sashi, yanayin tsinke Daidaitaccen rufewa ko yanayin kayan aiki; sa'an nan kuma sake rarraba kayan maimakon rage duka sashin a makanta
Bakin ciki ko rauni tsinke Narkar da zafi da yawa, rashin isassun abu a walda, ƙwanƙwasa lissafi mara dacewa, wuce gona da iri ko busawa da wuri Sashin walda, matsayin parison, ainihin zafin jiki, lokacin busawa, yanayin kayan aiki da aka yarda Maido da tsayayyen thermal da tushen lokaci; duba mold kafin ƙara duniya nauyi
Yanke-kashe yanke ko tsaga Sanyi parison, kaifi ko lalacewa, tsutsa mai sauri, kusa da m, rashin daidaituwa Sashe tare da walƙiya har yanzu haɗe, yanke wuri, motsin ƙira da gefen kayan aiki Gyara lalacewa/daidaitawar jiki kuma tabbatar da jeri-kusa da mold; yi kawai sarrafa thermal canje-canje
Kaurin bango mara daidaituwa Matsayin bayanin martaba, mutuƙar tsakiya, sag na parison, fitarwa mara ƙarfi, canjin ƙira, sanyaya asymmetric ko shimfiɗa Kafaffen taswirar bango akan zagaye da yawa, nauyin sashi, ra'ayin rata da gefen lahani Rarrabu buƙatun bayanin martaba na gida daga asymmetry na injina; yi amfani da taswirar bangon da aka amince
Ƙananan sasanninta, kafada ko hannu Babban shimfidar wuri, parison yayi ƙanƙanta ko ba daidai ba, rashin isassun kayan aiki, tuntuɓar wuri Mafi ƙarancin wurin bango, diamita/tsawon parison, jeri-zuwa-bangare Sanya abu a yankin da ake buƙata kuma tabbatar da matsayin parison kafin ƙara yawan nauyi
Parison sag ko drawdown Ƙarfin narkewar ƙanƙara, zafin jiki mai yawa, dogon lokacin rataya, babban parison, halayen guduro Tsawon Parison da siffa akan lokaci, ainihin yanayin narkewa, lokacin jujjuyawa/canja wuri Rage lokacin mara tallafi ko daidaita narkewa da fitarwa a cikin ingantaccen taga tsari
Parison curl ko hooking Mutuwar rashin daidaituwar zafin jiki, rashin daidaituwa, gurɓatawa a bakin mutun, rashin daidaituwa Jagoran lanƙwasa, yanayin zafi, yanayin mutu-lebe da ainihin yankin kai Bada barga mai dumi; dubawa da tsaftacewa ta amfani da hanyar da aka yarda; daidai jeri maimakon ramuwa a mold
M parison, narke karaya ko orange kwasfa Rashin kwanciyar hankali na gudana, rashin dacewa da juzu'i, yanayin zafin jiki, ƙasa mai mutu ko ƙaƙƙarfan ƙura ko iska mara kyau Ko rashin ƙarfi ya wanzu akan parison kyauta, ƙimar extrusion, saman mold da huluna Gano parison da asalin mold; dawo da tsarin extrusion zuwa cikin barga taga
Kumfa ko babu Danshi/condensation, iskar gas, mara kyau hadawa, yayyo abu/lalata, gurɓata Sarrafa kayan aiki, yanayin hopper/maƙogwaro, ƙirar kumfa, buƙatun guduro da daidaiton narkewa Cire sanadin sarrafa kayan; tabbatar da haɗawa da yanayin kayan aiki kafin ƙara matsa lamba na baya
Baƙar fata ko alamun kuna Ragewar guduro, matattun tabo, gurɓataccen regrind, yawan lokacin zama ko rufewa/farawa mara kyau Lokacin da specks ya fara, launi/regrin kuri'a, yanayin tsaftacewa, tarihin zafin jiki da lokacin raguwa Keɓe abubuwan da ake zargi da bin ƙa'idar tsarkakewa/tsaftacewa; cire tushen lalacewa
Rasu Lines ko streaks Lalacewa/datti mutu leɓe, gurɓatacce, gurɓataccen abu, launi mara daidaituwa ko kwarara Ko an daidaita layin a kusa da parison, binciken mutuwa-lebe da tarihin canjin abu Kare madaidaicin saman kuma tsaftace ta hanya; daidaita kayan abu daidai ko lalacewa
Rashin cikar bugu ko mara kyau daki-daki Ƙuntatacce / rashin isassun iska, ɗigogi, rashin iska mara kyau, sanyi mai sanyi, lokaci ko gajeriyar parison Iska mai shigar da na'ura yayin busawa, busa-pin hatimi, iska da yanki na bakin ciki/wanda ba a gama ba Maido da isar da iskar da iska; tabbatar da kama parison da asalin yanayin zafi
Busa-fita Rauni ko yanke parison, tsunkule mara daidai, matsi mara nauyi, tsayin daka, gajeriyar parison ko busa mai tsanani Asalin gazawa, kama parison, yanayin tsunkule, taswirar bango da rufewa Gyara gazawar jiki ta farko; kar a ɓoye ta ta ƙara faɗin nauyi
Warpage, rocker kasa ko m wuya Rashin isasshen sanyi ko rashin daidaituwa, tashar da aka toshe, zafi mai narke, fitar da wuri, rarraba kayan da bai dace ba Samar da/dawo da ruwa, yanayin zafin rami, lokacin sanyaya da canji bayan fitarwa Mayar daidaitaccen cirewar zafi; sannan duba lokacin zagayowar da rarraba bango
Leak ko gaza gwajin aikin aiki Rauni-kashe, ramuka, bangon bakin ciki, ƙare wuyansa, lalacewa, gurɓatawa ko saitin gwaji Alama daidai matsayin gazawar; sashin sashin; tabbatar da tester da datsa yanayin Bi diddigin ɗigon zuwa matakin da ya samo asali kuma maimaita ƙayyadadden gwajin bayan gyara

Abu da narke lahani: bi da yawa a gaban inji

Lokacin da lahani ya fara bayan guduro, masterbatch ko regrind canji, adana lakabi da samfurori kafin daidaita kayan aiki. Yi rikodin darajar guduro, kuri'a, rabon launi, tushen regrind, allon niƙa, yanayin ajiya da lokacin canji. Gurɓataccen gauraya na iya haifar da baƙar fata, ɗigo, kumfa, layukan mutu, rashin walda mara kyau da extrusion mara ƙarfi. Daidaita ɗaya ba zai iya gyara dukkan su ba.

Danshi baya daya a fadin kayan. Bi buƙatun kulawa da busasshen mai siyarwar mai siyarwa maimakon ɗauka cewa kowane guduro gyare-gyare yana buƙatar magani iri ɗaya. Kwangila akan kayan sanyi ko a yankin ciyarwa na iya haifar da matsala koda lokacin da polymer ba a bushe ba. Jagoran magance matsalar LyondellBasell yana gano ƙazanta da narke rashin daidaituwa tsakanin yiwuwar kumfa da lahani na bango.

Baƙar fata, hayaki da kayan konewa

Da farko ƙayyade ko an daidaita lahani zuwa hanyar guda ɗaya ko kuma an rarraba shi ba da gangan ba. Tsayayyen layi na iya nuna wurin mutuwa/wurin kai. Bazuwar tabo na iya biyo bayan gurɓataccen guduro, sake niƙa ko ƙasƙantar kayan da aka saki daga matattu. Bitar dogon tasha, yanayin zafi mai zafi, farawa da bayanan rufewa, sannan yi amfani da na'ura- da hanyar tsarkakewa ta hanyar guduro. Kada a goge madaidaicin saman saman da kayan aikin da ba a yarda da shi ba.

Launuka masu launi da haɗuwa mara daidaituwa

Bincika ko ɗigon ya biyo bayan canjin abu, ƙaramar ƙima mai yawa, katsewar ciyarwa ko ƙayyadadden matsayi na mutuwa. Bincika rikodin allurai da haɗakarwa kafin ƙara kuzarin haɗuwa. Ƙarin matsa lamba na baya zai iya inganta haɗuwa a wasu matakai, amma kuma yana iya ƙara zafi mai zafi da lokacin zama. Madaidaicin amsa ya dogara da extruder, guduro da kafaffen taga tsari.

Kinggle extrusion blow molding machine with guarded molding area and operator control panel
Binciken lahani yakamata ya haɗa abubuwan lura na zahiri a na'ura tare da bita girke-girke, yanayin amfani da auna sakamakon sashi.

Lalacewar Parison da kaurin bango mara daidaituwa

Parisson ya riga ya canza kafin mold ya rufe. Kumburin mutu yana ƙara girman sa yayin da yake fita kayan aiki; nauyi da ƙananan ƙarfin narkewa na iya jawo shi zuwa ƙasa; zafin jiki da kwarara iya bambanta kewaye da kewaye. 2025 binciken bude-hannu akansamuwar parison ta amfani da bayanan aiwatar da extrusionHakanan yana ɗaukar kumburi, raguwa da rarraba zafin jiki azaman mahimman abubuwa. Wannan shine dalilin da ya sa taswirar bangon da aka gama ya fi amfani fiye da matsakaicin kauri guda ɗaya.

Lokacin da bango ya zama bakin ciki a gefe ɗaya

Auna ma'auni iri ɗaya akan sassa da yawa a jere. Idan gefen bakin bakin ciki ya tsaya tsayin daka dangane da mold, duba mutun tsakiya, matsayi, sanyaya wuri da tuntuɓar parison na farko. Idan yana juyawa ko motsi, bincika kwanciyar hankali na extrusion, daidaiton kayan aiki da amsawa. Kar a ɓata rashin daidaituwar injina tare da bayanin martaba mai rikitarwa sai dai idan an kawar da dalilin jiki.

Lokacin da kusurwa, kafada, hannu ko kasa ya zama bakin ciki

Waɗannan fasalulluka sun shimfiɗa parison fiye da bango madaidaiciya. Tabbatar da cewa parison ya kai daidai tsayi da matsayi a kusa da mold. Sannan daidaita sashin kauri da aka tsara tare da fasalin da ake buƙata. Kinggle'sshirye-shiryen parison da jagorar kauriyayi bayanin matsayin bayanin martaba, buɗewar gida da ma'auni gabaɗaya daki-daki.

Lokacin da kauri ya canza daga zagayowar zuwa zagayowar

Bayanan martaba ba shine gyaran farko na tsari mara tsayayye ba. Kwatanta ainihin zafin jiki, fitarwar extrusion, harbin tarawa ko matsayi inda ya dace, tsayin parison, halayen hydraulic da umarnin mutuwa-rabo/amsa. Tabbatar da tsari kafin gyara maki da yawa. Ajiye girke-girken da aka karɓa azaman ingantaccen bita don ƙungiyar ta iya juyar da canjin da bai yi nasara ba.

Filashin walƙiya, gazawar kashe-kashe da ɓangarori

Filashi shine abu na waje da aka ƙera, yawanci a kusa da layin rabuwa, wuya da tsunkule ƙasa. Wasu walƙiya suna da alaƙa zuwa gyare-gyaren busa extrusion kuma ana cire su a ƙasa. Lalacewar ya wuce kima, asymmetric ko walƙiya mara ƙarfi wanda ke shafar datsa, ingancin walda, nauyi, ƙulli ko amincin zagayowar.

Karanta tsarin walƙiya a matsayin shaida

  • Filanci ko'ina:kwatanta nauyin sashi, girman parison, kammala-ƙusa-ƙusa da yanayin matsa.
  • Filashi a gefe guda:duba jeri na mold, daidaitacce, yanayin kayan aiki da jeri na parison.
  • Filashin yana ƙara kauri akan lokaci:bita drift thermal drift, harbi/fitarwa drift, lalacewa da na'ura mai aiki da karfin ruwa yanayin.
  • Filanci yaga weld yayin datsa:duba tsinke-kashe lissafi, lalacewa, rufewa da datsa tsarin kafin canza yanayin zafi.

Weld na bakin ciki, tsagewar walda da yanke parison suna da nau'ikan gazawa daban-daban. Jagorar LyondellBasell ya raba waɗannan matsalolin da ba su da ƙarfi saboda yuwuwar magunguna na iya nunawa a wasu kwatance. Rike filasha a haɗe zuwa samfurin da ya gaza har sai an rubuta asalin gazawar.

Bincika ɗigon ruwa zuwa matakin kafawa

Alama wurin ɗigo daga mai gwadawa, sa'an nan kuma raba sashin idan tsarin inganci ya ba shi damar. Zuba ruwa a ƙasan walda yana jagorantar ƙungiyar zuwa ga tsinkewa, sanya kayan abu da sanyaya. Kumburi a cikin jiki yana kaiwa zuwa kumfa, gurɓatawa, layin mutu ko bakin bango na gida. Zubewar wuya na iya haɗawa da samuwar ƙarewa, datsa, saka matsayi ko na'urar gwajin. Tabbatar da mai gwada zubewar tare da sanannen tunani kafin canza tsarin gyare-gyare.

Lalacewar saman: raba parison daga mold

Kula da parison kyauta lafiya daga wajen yankin da aka gadi. Idan layi ko rashin ƙarfi ya riga ya wanzu kafin mold kusa, bincika abu, narke kwanciyar hankali da yanayin mutu. Idan parison ya yi kama da karbuwa amma saman da aka gama ya dushe, rami ko rashin daki-daki, duba saman mold, hushi, hurawa, zafin jiki da natsuwa.

Orange kwasfa da m surface

Yadudduka masu yuwuwa sun haɗa da ƙaƙƙarfan kwararar parison, ƙarancin iska mai kyau, ƙarancin isar da iska ko ƙuntataccen isar da iska, yayyafawa a kusa da fil ɗin busa, parison sanyi ko lallausan wuri. Duba matsa lamba a na'ura a lokacin bugu; nunin kwampreso a wani wuri a cikin masana'anta baya tabbatar da cewa matsa lamba da kwarara sun isa ga ƙirar a lokacin da ake buƙata. Kinggle'sjagorar tsara kayan aikiyana rufe iska da hanyar sanyaya daga samar da shuka zuwa haɗin injin.

Die Lines da kafaffen streaks

Alama matsayi na ratsi a kusa da sashin kuma kwatanta shi da parison. Idan ya tsaya a kafafe, duba madaidaicin hanyar kwarara bayan madaidaicin kashewa da keɓewa. Ƙaƙwalwar lebe na mutuwa na iya haifuwa akan kowane zagayowar. Lalacewa ko gurɓataccen guduro kuma na iya shiga cikin kai kuma ya saki na ɗan lokaci. Dole ne tsaftacewa ya kare madaidaicin saman kuma ya bi hanyar da aka kawo.

Lalacewar sanyaya, yaƙe-yaƙe da ɓacin ƙira

Warpage yakan zama bayyane kawai bayan fitar da shi. Kwatanta sashin nan da nan bayan buɗe gyare-gyare, bayan datsa da kuma bayan ƙayyadadden lokacin sanyaya. Ƙarƙashin dutsen dutse, wuyan hannu ko juzu'i mai girma na iya biyo bayan rashin isasshen sanyaya, yanayin zafi mara daidaituwa, tashar ruwa da aka toshe, zafi mai zafi, sarrafa wuri ko rarraba bango mara daidaituwa.

Yi rikodin samarwa da dawo da zafin jiki, matsa lamba da - lokacin da akwai kayan aiki - kwarara don da'irar ƙirar ƙira. Tabawa ba ingantaccen ma'aunin zafin jiki ba ne kuma baya bayyana tashoshi da aka iyakance. Idan gefe ɗaya na ɓangaren ya canza yayin da samar da shuka ya tsaya tsayin daka, bincika mahallin gida, haɗi, tashar da yanayin ƙira.

Hangen masana'anta:karuwar lokacin sanyaya na iya ɓoye matsalar canja wurin zafi yayin rage fitarwa. Da farko tabbatar da cewa hanyar ruwa da aka tsara tana aiki. Sannan inganta sake zagayowar a cikin ingantaccen taga mai inganci.

Injin, HMI da masu amfani da kayan aiki kafin daidaitawa

HMI yana nuna buƙatun, ra'ayi, yanayin jeri da ƙararrawa. Ba ya tabbatar da cewa bawul ɗin ya motsa, iska ta kai ga busa fil ko ruwa ya gudana ta cikin tsari. Karanta ƙimar saiti da ainihin ƙimarsa azaman biyu, sannan kwatanta allon tare da sakamakon jiki.

Lura Abin da zai iya raba Duba lafiya na gaba
Ƙimar saita yanayin zafi tana da ƙarfi amma ainihin ƙima tana ja da baya Batun girke-girke tare da firikwensin, hita, sanyaya ko batun sarrafawa Bitar yanayin fitarwa, tarihin ƙararrawa da hanyar duba wutar lantarki/zazzabi mai izini
Isar da iska na yau da kullun ba ya aiki amma lahani yana bayyana yayin busawa Matsi na tsaye tare da matsi mai tsauri/ iyakancewar kwarara Rikodi matsa lamba na inji-shigarwa yayin buƙatar masana'anta lokaci guda
Umurni yana canzawa amma parison ko sashi baya amsawa Umurnin girke-girke tare da actuator, bawul, daidaitawa, manne ko batun amsawa Kwatanta umarni da martani, sannan haɓaka ƙarƙashin tsarin kulawa
Ƙararrawa yana maimaitawa a mataki guda na sake zagayowar Lamarin bazuwar tare da bacewar izini, matsayi ko yanayin lokaci Ajiye ƙararrawar farko kuma duba abubuwan da ke da alaƙa da yanayin jiki
Lalacewar ta fara bayan an ɗora kayan girke-girke da aka ajiye Laifin injin tare da girke-girke/mold/ rashin daidaituwa na kayan aiki Kwatanta bita, raka'a, ƙirar ƙira da tushe mai kariya ba tare da sake rubutawa ba

Yi amfani daKinggle HMI saituna da jagorar ƙararrawadon tsari mai tsari. Idan matsalar ta hada da yoyo, yanayin zafi, mai datti, ƙuntataccen sanyaya ko ƙararrawa mai maimaitawa,jerin abubuwan kulawa na rigakafiyana taimakawa haɗa ingancin samfur tare da yanayin injin.

Kinggle accumulator extrusion blow molding machine showing die head guards and control cabinets
Nau'in inji, shugaban mutu, mold, sarrafawa da mataimaka suna canza hanyar magance matsala daidai; yi amfani da takamaiman takaddun aiki.

Duban masana'anta: gina rikodin lahani wanda wani motsi zai iya amfani da shi

"Madaidaicin zafin jiki kuma yanzu mafi kyau" ba rikodin sake bugawa bane. Logo mai amfani yana haɗa ɓangaren da ake zargi zuwa lokaci, yanayin inji da ingantaccen sakamako. Hoton lahani tare da ma'auni ko wuri mai alama lokacin aiki, kuma kiyaye ingantaccen samfurin da aka yarda don kwatantawa.

Filin yin rikodi Abin da za a kama Me ya sa yake da mahimmanci
Shaida Kwanan wata/lokaci, inji, mold, rami/kai, bita samfurin, mai aiki da motsi Yana nuna ko laifin ya biyo bayan kayan aiki, kayan aiki ko mika hannu
Kayan abu Matsayin guduro / kuri'a, masterbatch, tushen regrind da rabo, lokacin ɗorewa Yana haɗa lahani tare da canjin abu ba tare da zato ba
Alama Madaidaicin wuri, mita, sake zagayowar farko, hoto da samfurin da aka riƙe Yana raba ƙayyadaddun lahani daga bambance-bambancen tsari
Yanayin tsari Bita na girke-girke, ainihin yanayin zafi, nauyin sashi, lokacin sake zagayowar, kallon parison/ harbi da ƙararrawa ta farko Yana kiyaye tushen tushe kafin gyare-gyare yana goge shaida
Abubuwan amfani Injin-shigar iska da yanayin ruwa yayin samarwa; dacewa yanayin hydraulic Yana bayyana matsalolin shuka da aka raba ko kawar da zafi
Canjin sarrafawa Tsohuwar ƙima, sabon ƙima, dalili, mutum da lokaci Yana hana canje-canje da yawa a lokaci guda daga ɓoye sanadin
Tabbatarwa Ƙididdigar sake zagayowar da aka ayyana ta hanyar shuka, taswirar bango, nauyi, girma da gwaje-gwajen aikin da ake buƙata Yana tabbatar da ko gyaran ya inganta ainihin abin da ake bukata

Lokacin da za a daina daidaitawa da haɓaka

  • Mai gadi, kulle-kulle, tsayawar gaggawa ko iko mai haɗari-makamashi baya aiki kamar yadda aka yi niyya.
  • Ana zargin wani karo na inji, motsi mara tsammani, yanayin wutar lantarki mai zafi, ɗigon ruwa ko ɓarna matsi.
  • Irin wannan lahani ya kasance bayan an tabbatar da kayan, kayan aiki da ingantaccen tsarin girke-girke an dawo dasu.
  • Umurni da ainihin martani ba su yarda ba, ko tsarin ba ya amsa da tsinkaya ga canji mai sarrafawa.
  • Ana buƙatar gyaran kayan aiki, daidaitawa, canjin shirin ko aiki a waje da taga tsari da aka amince.

Hana maimaita lahani yana farawa kafin ƙaddamar da na'ura

Don sabon injin gyare-gyaren extrusion ko sabon ƙira, ayyana shaidar karɓa kafin gwaji. Samar da zanen ɓangaren, darajar guduro, nauyin manufa, wurare masu mahimmanci na bango, wuyansa da ma'auni gabaɗaya, shirin datsa, gwajin ɗigo ko matsa lamba, ma'auni na gani, manufa fitarwa da kayan amfanin shuka. Rahoton gwaji mai amfani yana haɗa samfuran da aka yarda da su zuwa ainihin ƙira, kayan aiki da bita na girke-girke.

Kananan kwantena da manyan ayyuka na iya dacewa da am extrusion busa gyare-gyaren inji. Manyan sassa ko nauyi na iya buƙatar waniaccumulator busa gyare-gyaren inji. Zaɓin daidai ya dogara da ɓangaren da tsarin aiwatarwa, ba sunan lahani kaɗai ba. Shiga Kinggle'sbusa gyare-gyare aikace-aikaceko aika ainihin bayanin samfurin don takamaiman aikin tattaunawa.

Tambayoyin da ake yawan yi

Wadanne lahani ne na yau da kullun na extrusion busa gyare-gyare?

Lalacewar gama gari sun haɗa da walƙiya da yawa, rauni ko yanke tsinke, kauri mara daidaituwa, kauri na bango, sasanninta na bakin ciki, sag ko murɗa, narke karaya, kumfa, baƙar fata, layukan mutu, busawa da bai cika ba, busa-fitowa, wargaɗi da leaks.

Me ke haifar da kaurin bango mara daidaituwa a cikin gyare-gyaren busa?

Dalilai masu yuwuwa sun haɗa da matsayin bayanin martaba, mutuƙar tsakiya, sag na parison, extrusion mara ƙarfi ko girman harbi, daidaitawar ƙira, sanyaya mara daidaituwa da adadin shimfiɗar da sashin lissafi ke buƙata.

Ta yaya za ku rage walƙiya a cikin gyare-gyaren busa extrusion?

Da farko duba inda walƙiya ya auku, nauyin sashi, jeri na parison, ƙayyadaddun ƙayyadaddun ƙayyadaddun ƙayyadaddun ƙira, ɗabi'ar matsawa, daidaitawa da yanayin kashewa. Gyara kuskuren rufewa ko kayan aiki kafin canza nauyin ɓangaren duniya.

Me yasa akwai kumfa a cikin abin da aka ƙera?

Dalilai masu yuwuwa sun haɗa da gurɓataccen ruwa ko danshi, iskar gas, rashin isasshen narkewa, ɗigon abu, gurɓataccen abu da gurɓatawa. Bincika buƙatun guduro da hanyar abu kafin canza tsarin.

Shin shirin parison zai iya gyara kowane lahani na bango?

A'a. Shirye-shiryen Parison ba zai iya dogaro da dogaron gyara kuskuren mutun ba, extrusion mara ƙarfi, lalata kayan aiki, sanyaya mara kyau, matsayi mara kyau ko injin kunnawa mara kyau.

Menene ya kamata a fara canzawa yayin warware matsalar gyare-gyare?

Da farko maidowa da tabbatar da ingantaccen kayan, girke-girke, mai amfani da tushen yanayin inji. Bayan gano mafi yuwuwar Layer, canza canjin sarrafawa guda ɗaya kuma maimaita ma'aunin sashi iri ɗaya.

Me yasa irin wannan lahani ke dawowa akan wani canji?

Lalacewar mai maimaitawa sau da yawa yakan dawo lokacin sake fasalin girke-girke, sauye-sauyen kayan aiki, karatun kayan aiki, ƙararrawa da ayyukan gyara ba a rubuta su akai-akai. Rubutun lahani da aka raba tare da tushe mai kariya suna sa tsarin maimaituwa.

Bayanan fasaha

Labarai masu alaka
Ka bar min sako
X
Muna amfani da kukis don ba ku ingantaccen ƙwarewar bincike, bincika zirga-zirgar rukunin yanar gizo da keɓance abun ciki. Ta amfani da wannan rukunin yanar gizon, kun yarda da amfaninmu na kukis. takardar kebantawa
ƘiKarba